I have an old set of bubblebags and a new set of Sprung bags...there exactly the same except for the pretty colors of the bubblebags...So why pay for the colors?
Which side did you guys use as the inside?
I almost bought a set of these, the 1680D Nylon used is very durable and hard-wearing. The one thing I'd have hoped to have seen was at least double-stitching around the screen..........unless there is a seam that's hidden in the pics I've seen?
In general though they look to be among the best bags I've seen on ebay though and at a price that doesn't break the bank if you're on a budget
we just gave a new 5 bag/5gallon set their 1st run last night, they aren't Bubbleman's, these are what you might term as 'mid-priced ebay' lol
Other than the 220mic work bag, the sizes are 160, 120, 73 and 20 (although I often doubt the actual size of cheap bags, it's probably 25mic? )
These are not the cheap bags...there identical to Bubble bags...I have a set of each, the stiching is the same the screens are also the same sizes..
We made the mistake of tossing in a family size Quality Street tin full of dry trim with a lot of powdered leaf material so it's all really green. Nonetheless the frozen fresh trim was plentiful in resin so we have an end product that looks crap but is still miles better than street kAk (soap)
krk - that stuff looks ok man, can I ask what bag that came from?......I'll hazard a guess at the weight of those 4 pieces at around a half oz?
No way dude thats 85grams...
ace - welcome to the world of bubble my friend , I know you won't regret your purchase!. When we got ours, our first thought was "we shoulda got a set years ago!"
Sand....lol!, it's all in the press dude!, some say bursting the trichrome heads produces a different high. I love home made finger/hand rubbed tho, the softer and shinier the betterHard dried out "sand" is just that...There is a transformation when hash is heated and worked it melts together and becomes a nice soft black bar/ball...charas.